1 kg of mixed pins - solder remover, gold, palladium and silver recovery - part 2
Переглядів 3 тис.11 місяців тому
In this video I will show you how: - remove solder @francois-pellier - recover gold - recover palladium - recover silver
1 kg of mixed pins - solder remover, gold, palladium and silver recovery - part1
Переглядів 3,7 тис.11 місяців тому
In this video I will show you how: - remove solder @francois-pellier - recover gold - recover palladium - recover silver
4.4 kg Ceramic CPUs and ICs - Precious metals recovery
Переглядів 10 тис.Рік тому
How to get Gold and silver from ceramic CPUs and ICs. Special thanks to Venca Bílek for 2 CPUs :-)
Rags - Gold recovery
Переглядів 2,7 тис.Рік тому
How to get gold from rags from the gold paint used in the glassworks.
Backplane boards - Gold recovery
Переглядів 7 тис.Рік тому
How to get gold from Backplane boards.
6 kg of Gold fingers - Gold recovery
Переглядів 37 тис.Рік тому
How to get gold from gold fingers (6 kg).
Dental scrap - Precious metals recovery
Переглядів 3,4 тис.Рік тому
How to get silver, palladium and gold from Dental scrap.
1 kg mix of metal transistors - Gold recovery
Переглядів 19 тис.2 роки тому
How to get gold from mix of white and gold transistors.
Ceramic ICs - Gold recovery
Переглядів 8 тис.2 роки тому
How to get gold from ceramic ICs.
1 kg of pins from Kontakta DS 1582 264 5 - Gold recovery
Переглядів 43 тис.3 роки тому
How to get gold from 1 kg pins.
Electrical switches and auxiliary contacts - silver recovery
Переглядів 41 тис.3 роки тому
Processing of silver contacts on a copper base. - Where these contacts are located. - How to get to them. - How to process them. - How to melt silver in an induction furnace.
400 keyboards - Silver recovery
Переглядів 39 тис.3 роки тому
How much silver is in 400 keyboards?
BGA chips (bottoms) - Gold recovery by stripping agent
Переглядів 33 тис.4 роки тому
This video is a test of recycling gold from the bottoms of BGA chips.
Low-grade material - Gold recovery by stripping agent
Переглядів 24 тис.4 роки тому
Low-grade material - Gold recovery by stripping agent
Test non-functional LCD for Cubot P20
Переглядів 1,7 тис.4 роки тому
Test non-functional LCD for Cubot P20
Airshow CHEB 2017
Переглядів 1,1 тис.5 років тому
Airshow CHEB 2017
MLCC's from Pentium 4 - Experiment - PM content
Переглядів 13 тис.5 років тому
MLCC's from Pentium 4 - Experiment - PM content
Cheap furnace for silver/gold melting - DIY
Переглядів 36 тис.5 років тому
Cheap furnace for silver/gold melting - DIY
Sockets Tesla TX 787 5401 - Gold recovery
Переглядів 6 тис.5 років тому
Sockets Tesla TX 787 5401 - Gold recovery
FRB connectors new, female - Gold recovery
Переглядів 9 тис.5 років тому
FRB connectors new, female - Gold recovery
URS male old type - Gold recovery
Переглядів 7 тис.5 років тому
URS male old type - Gold recovery
URS female old type - Gold recovery
Переглядів 13 тис.5 років тому
URS female old type - Gold recovery
IC chip Motorola MC3416L - Gold recovery
Переглядів 46 тис.5 років тому
IC chip Motorola MC3416L - Gold recovery
IC chips - Gold recovery (incinerating)
Переглядів 557 тис.5 років тому
IC chips - Gold recovery (incinerating)
Relays mix - silver, palladium and gold recovery
Переглядів 84 тис.6 років тому
Relays mix - silver, palladium and gold recovery
Relays National AE1324 - Gold recovery
Переглядів 31 тис.6 років тому
Relays National AE1324 - Gold recovery
Connectors DS 1582 264 5 - Gold recovery (surprise)
Переглядів 22 тис.6 років тому
Connectors DS 1582 264 5 - Gold recovery (surprise)
URS connectors male - Gold recovery
Переглядів 10 тис.6 років тому
URS connectors male - Gold recovery
Gold melting - 1/4 kg (8 oz)
Переглядів 10 тис.6 років тому
Gold melting - 1/4 kg (8 oz)

КОМЕНТАРІ

  • @radiocomponent
    @radiocomponent 15 годин тому

    Sodium pyrosulfite (Na2S2O5) stimulates the development of allergic reactions and causes diseases of the gastrointestinal tract. Releases toxic gas on contact with acids. If in contact with eyes, may cause eye damage. But this does not prevent this chemical compound from not only releasing gold from solution, but also being a food additive E223. Пиросульфит натрия (Na2S2O5) стимулирует развитие аллергических реакций, вызывает заболевания желудочно-кишечного тракта. При контакте с кислотами выделяет токсичный газ. При попадании в глаза может вызвать повреждение глаз. Но это не мешает этому химическому соединению не только выделить золото из раствора, но и быть пищевой добавкой Е223.

  • @user-yu5ol5vz7q
    @user-yu5ol5vz7q 21 годину тому

    Лайк тебе и подписка 👍🔥

  • @SunRabbit
    @SunRabbit 2 дні тому

    Podle mne jste nedostal vsechno Stribro hned pri prvnim postupu. Na tech folii nema spravne zustat nic krome nepatrnyho a pruhlednyho stinu tech puvodnich nanosu. Ja jsem videl video kdysi davno kde pouzival varici kyselinu dusicnou aby docilil prave toto. Mimo jiny, KDE jste sehnal dusicnou? Ja mam folie z asi 1000 klavesnic (bedna asi 60 x 40 x 40) a ja asi to cely spalim, pak odstranim ten popel s tetrachlorem, pak to vyredukuju elektrolyticky. Jeste se ale musim poradit s jednim profesorem chemie ohledne nejlepsiho postupu.

  • @YourDailyVideoNews
    @YourDailyVideoNews 8 днів тому

    Great video ‼️‼️

  • @coinkiller5495
    @coinkiller5495 8 днів тому

    And it will go green and you can reuse it time and time again if slowdowns just add some more HC it will go dark green and put all kinds of boards in with gold flashing on it floats of and strain gold off and do it again and again put gold fingers in and over night gold floats of copper chloride two it’s called

  • @coinkiller5495
    @coinkiller5495 8 днів тому

    AP is hydrochloric acid and food grade peroxide for shop put 50 mill in 2 litres of hc

  • @YourDailyVideoNews
    @YourDailyVideoNews 8 днів тому

    Cool Video - please do more 👍👍👍

  • @IsmetBiljali-vg4hu
    @IsmetBiljali-vg4hu 14 днів тому

    Perfect

  • @IsmetBiljali-vg4hu
    @IsmetBiljali-vg4hu 14 днів тому

    Very nice work

  • @andrebattis9410
    @andrebattis9410 14 днів тому

    Good job

  • @andrebattis9410
    @andrebattis9410 14 днів тому

    Second AR you should added sulfuric acid to dissolve tin or lead

  • @patrick8198
    @patrick8198 20 днів тому

    24k pure nice gold ❤😂

  • @patrick8198
    @patrick8198 20 днів тому

    Wow!👀🤩….. That is a nice lick👅❤️😂

  • @vanquynguyen8298
    @vanquynguyen8298 22 дні тому

    Hơn 1 kg các chân mạ vàng này ta thu được 6,5 g vàng , cũng nhiều hơn so với lượng vàng có trong IC thông thường ( không kể những con chip máy tính ) ?

  • @patrickwilliams4613
    @patrickwilliams4613 Місяць тому

    Nice video good job

  • @knowldedge5012
    @knowldedge5012 Місяць тому

    how do you separate capacitors from the pins?

  • @okboomer6201
    @okboomer6201 Місяць тому

    Next time talk a bit so we know WTF you are doing

  • @ScienceInspiration-ot1le
    @ScienceInspiration-ot1le 2 місяці тому

    Hello can i know whats mean denox mean .if use any chemical for denox

  • @goldandsilverminingintheci8942
    @goldandsilverminingintheci8942 2 місяці тому

    I once did a small moving job for a handful of gold crowns. Worked for me!

  • @coinkiller5495
    @coinkiller5495 2 місяці тому

    One thing bro you had to denox?? How much nitric did you use?? If you start with few mills at a time on heat and with lid on reaction stops put few more mills in until it’s resolved and the more legs you remove before you start you will use less nitric because copper takes a lot of nitric and the more copper you need more liquid to dissolve the salts in but good job we’re is the water for SMB you drop gold you need double solution water???????

  • @coinkiller5495
    @coinkiller5495 2 місяці тому

    Hi moose coin killer from Australia here what I do with my chips first is I put in AP for few weeks or so and it eats all the magnetics out of the chips all the way up and inside 85% so less to eat away with expensive nitric great video should try it out and make a video on it

  • @NanamiKairyu
    @NanamiKairyu 2 місяці тому

    sulfic acid should be like 96% atleast 86 will not work actually(only little bit). It's long time taking, dangerous, also usage of acid is high. Only one bonus that gold not lost in the process like you can do when burning.

  • @user-db9yv7lu9v
    @user-db9yv7lu9v 2 місяці тому

    I think too much that the gold and pal from 7.5g (0.2g and 0.44?)

  • @lukasrosko1480
    @lukasrosko1480 2 місяці тому

    Chapem to spravne 200g pinou a jeden g zlata ? Cca 30e +- ?

  • @ezatsheshtawy9766
    @ezatsheshtawy9766 3 місяці тому

    Excellent ❤ ‏‪nice time

  • @otorejthar3474
    @otorejthar3474 3 місяці тому

    Hi Bohumil,I have question. How long did you soak the plates for? In your first step

    • @BohumilGraman
      @BohumilGraman 3 місяці тому

      Until all the metals are etched away.

    • @otorejthar3474
      @otorejthar3474 3 місяці тому

      How I can you contact (pm)? FB or something. I need your help

    • @otorejthar3474
      @otorejthar3474 3 місяці тому

      How I can contact you private? Can you give me email? I have any more questions.

  • @henrykmielczarek3189
    @henrykmielczarek3189 3 місяці тому

    Jaki sens ważyć z metalem w 0,55 min.

    • @BohumilGraman
      @BohumilGraman 3 місяці тому

      Abych měl alespoň přibližnou představu, kolik HNO3 budu potřebovat.

  • @user-lm5ix3ce5l
    @user-lm5ix3ce5l 3 місяці тому

    I feel like this was not done as efficient as possible. 99 cpus and only 0.6 grams of gold?!

  • @spanek158
    @spanek158 4 місяці тому

    Paráda. A tu indukční pícku jste si dělal? Roztaví i zlato?

  • @user-lm3nd5ow9j
    @user-lm3nd5ow9j 4 місяці тому

    How much urea used in one litre aqua regia

    • @BohumilGraman
      @BohumilGraman 3 місяці тому

      As much as removes the remaining nitric acid. You know how much is left?

  • @henrykmielczarek3189
    @henrykmielczarek3189 4 місяці тому

    Liczyłem na ok 12 g

    • @BohumilGraman
      @BohumilGraman 4 місяці тому

      Je to mix, záleží na podílu zlacených a nezlacených tranzistorů.

  • @fightington
    @fightington 5 місяців тому

    Anything with a high frequency of contacting - look for platinum/paladium- its used cause it doesnt wear out like gold/silver - lasts a lot longer

  • @Edward-ju1vj
    @Edward-ju1vj 6 місяців тому

    There is no way he got that much from 1kg. You get more like 1 gram. I'm not sure exactly where but he spiked it somewhere along the line there's no way you can get that much from 1 kg!!!!

    • @BohumilGraman
      @BohumilGraman 5 місяців тому

      Another smart guy without a single experience with these connectors, but who knows exactly what is or is not possible. Get them (the type is there) and then judge. Feel free to make your own video exposing me. In the Eastern Bloc, they used to make gold plated pins like that a lot. There are richer pins.

  • @Edward-ju1vj
    @Edward-ju1vj 6 місяців тому

    Lucky that the pin rack wasnnot glued to the board... I've never seen that.

    • @BohumilGraman
      @BohumilGraman 5 місяців тому

      In the vast majority of cases, it's not glued.

  • @stefanzivkovic714
    @stefanzivkovic714 6 місяців тому

    Nice video sir, can you tell me, how many karats did you get, what is the purity of this gold you made?

  • @lukasbaumgartner4303
    @lukasbaumgartner4303 6 місяців тому

    STO ROKOV KEĎ TO TAKTO BUDETE ZÍSKAVAŤ TAK MÁTE 20g zlata a nič z toho zabitý čas ale Číňania a pakistanci a Indovia majú čas na ťažbu zlata 😂😂😂😂😂😂😂😂😂😂

    • @BohumilGraman
      @BohumilGraman 5 місяців тому

      Fakt? Koukám profík :-) Určitě máte pravdu, jsem rád, že si to myslíte. :-)

    • @lukasbaumgartner4303
      @lukasbaumgartner4303 5 місяців тому

      @@BohumilGraman a vy tomu ešte veríte 😂😂😂😂 vlastne youtube ma vždy pravdu 😂😂😂😂😂

    • @BohumilGraman
      @BohumilGraman 5 місяців тому

      @@lukasbaumgartner4303 :-) Tohle není otázka víry ;-)

  • @MuzzammilHussainQureshi-qs1ix
    @MuzzammilHussainQureshi-qs1ix 6 місяців тому

    If there is 6 kg with finger then what will be the average with Ram?

    • @BohumilGraman
      @BohumilGraman 5 місяців тому

      I not understand you question

  • @Janezhallam
    @Janezhallam 6 місяців тому

    need gas mask with full face protection and rubber gloves, and also a environment suit.

  • @akgoldbear7669
    @akgoldbear7669 6 місяців тому

    I thought there was something wrong with my computer. The playback speed needs to be increased by 1.25. Will there be another part of the video about the palladium that was in your beaker? 😎

    • @BohumilGraman
      @BohumilGraman 5 місяців тому

      I tested it with DMG - no Pd :-(

  • @quinton3997
    @quinton3997 6 місяців тому

    Hard to believe there's that much gold in them

  • @devendraramnivasbaiddevend1763
    @devendraramnivasbaiddevend1763 6 місяців тому

    Not clear t in this video

  • @devendraramnivasbaiddevend1763
    @devendraramnivasbaiddevend1763 6 місяців тому

    Fake video

    • @BohumilGraman
      @BohumilGraman 5 місяців тому

      No :-) My video is not only one on UA-cam with this material.

  • @johannbackhus858
    @johannbackhus858 6 місяців тому

    Na konci pisete vynos z urs az 30g/kg. V inych videach uvadzate cca 9g/urs. Ktore typy su tak vynosne prosim? Dakujem a drzim palce 🙏🏻

    • @BohumilGraman
      @BohumilGraman 6 місяців тому

      To kdybych tušil, vždy je to překvapení :-)

    • @johannbackhus858
      @johannbackhus858 6 місяців тому

      @@BohumilGraman asi vtedy galvanizovali od oka a majster ked si odbehol na kafe,tak teraz mame o to vacsiu radost 😎

  • @ayhamhafez285
    @ayhamhafez285 7 місяців тому

    What is the idea from using the mentioned recipe to get rid off tin rather than using only HCl? I soak pcb in HCl with very good results,but I wonder why you use nitric and citric recipe,is there any advantage?

    • @BohumilGraman
      @BohumilGraman 6 місяців тому

      Po použití HCL je nutný mnohonásobný oplach, který v tomto případě zcela odpadá.

  • @delaem_zlato_
    @delaem_zlato_ 7 місяців тому

    Что-то маловато🤔, должно минимум 30 получится , я перерабатывал 2 килограмма взял 11.2 грамма золото ; 🤔🤔🤔 тоже обрезал с оперативной памяти только ...

    • @BohumilGraman
      @BohumilGraman 6 місяців тому

      Asi to nebude stejný materiál...

    • @delaem_zlato_
      @delaem_zlato_ 6 місяців тому

      @@BohumilGraman maybe another one , the material was all from RAM

  • @henrykmielczarek3189
    @henrykmielczarek3189 7 місяців тому

    co za bzdury żeby z 200gr styków ( miedz + srebro około 80 % ) wyszło 124 gr srebra > 95% bzdury , bzdury

    • @BohumilGraman
      @BohumilGraman 7 місяців тому

      Další profesionál, který rozumí všemu :-D Pokud bys koukal na video pořádně, viděl bys, že mnoho kontaktů bylo BEZ měděné osnovy - tedy celé stříbrné. Můžeš mi říct jediný rozumný důvod, proč bych dělal fake? :-)

  • @AB-mn2tx
    @AB-mn2tx 8 місяців тому

    Hi, great video. I am going to attempt this. What is AR ?

    • @BohumilGraman
      @BohumilGraman 7 місяців тому

      Aqua regia

    • @jonny1511
      @jonny1511 2 місяці тому

      @@BohumilGraman ist Salzsäure + Salpetersäure = Königswasser

  • @robertdelgado1385
    @robertdelgado1385 8 місяців тому

    Nice. Very organized and clear thoughts i like that. Would you be willing to accept material to process if we can both be profitable. I understand that for the prices of chems it would have to be profitable ill email you some possibilities

    • @BohumilGraman
      @BohumilGraman 7 місяців тому

      I'm sorry, but I have so much of my own material that I have to decline your offer.

  • @roymoreno7864
    @roymoreno7864 9 місяців тому

    This sucks you don't say anything about what your adding or how much to what your working with . So I dis you.

  • @denverDude-yj9kg
    @denverDude-yj9kg 9 місяців тому

    This is so fake! Max yield on what he SHOWED would be no kore than 6g, he added another 20 for melt… come on people wake up, there isnt that much gold on plating

    • @BohumilGraman
      @BohumilGraman 9 місяців тому

      Some pro again :-( Try to get this material first and then tell your "truths". In the Eastern Bloc, such gold plating was not uncommon.

    • @Edward-ju1vj
      @Edward-ju1vj 6 місяців тому

      Exactly right